1. 不需预制疲劳裂纹。
No fatigue precracking is required.
2. 疲劳裂纹的形成是该阶段最重要的特征。
The formation of fatigue cracks became the most important features in this stage.
3. 拍摄了热疲劳裂纹的形核、成长、连接过程。
The nucleation, growth and connection of fatigue cracks were photographed.
4. 叶片裂纹是疲劳裂纹,主要由交变应力引起。
They are fatigue cracks which is mainly caused by alternating stress.
5. 并讨论了疲劳裂纹的发生、扩展与组织的关系。
The relation between the extension of fatigue cracks and structure are discussed.
6. 建立了应变能与疲劳裂纹信号之间的数学模型。
Mathematic model between strain energy and tired flaw signals is established.
7. 介绍了复杂载荷下疲劳裂纹形成寿命预测的方法。WWW.WentiYi.COm
The methods of fatigue crack initiation life predictions under complex load are introduced in this paper.
8. 其疲劳裂纹的稳定扩展也较难形成典型的疲劳条带。
And formation of typical fatigue striation on fatigue crack steady propagation is difficult.
9. 提出了拉伸超载对疲劳裂纹扩展过程影响的一般机制。
A general mechanism of the effect of tensile overload on FCP behaviour is proposed.
10. 分析了冷扩张对疲劳裂纹尖端应力强度因子分布的影响。
The influence of cold expansion on the stress intensity factor distribution in crack tip was also analyzed.
11. 通过疲劳损伤准则,导出疲劳裂纹稳定扩展速率的计算公式。
The formula of the fatigue crack propagation rate was directly derived from the fatigue damage criterion.
12. 最后给出了根据钢的拉伸性能估算疲劳裂纹起始寿命的实例。
Finally, examples are given for predicting the fatigue crack initiation life from the tensile properties of steels.
13. 导致剥落的疲劳裂纹开始于表面缺陷和氮化层与心部交界处。
Cracks leading to spalling were initiated at surface defects and boundaries between nitriding layes and the core.
14. 疲劳裂纹的萌生和扩展是材料在变载荷作用下的主要失效形式。
The origination and propagation of fatigue crack in materials under variable load is the main style of failure.
15. 在实际使用中,在镀层的过渡段发生的疲劳裂纹会导致接耳断裂。
In service, fatigue cracking initiated at the plating runout led to lug fracture.
16. 本文对谱载荷下预测疲劳裂纹扩展的各种模型作了综合介绍及评述。
This paper gives a comprehensive introduction and review of the models for predicting fatigue crack growth under spectrum loadings.
17. 研究中应用了一种柔度法疲劳裂纹自动测量系统进行裂纹长度测量。
An automatic compliance crack length measurement system for fatigue crack propagation test was used in the experiments.
18. 在应力比,残余应力对疲劳裂纹扩展的影响方面获得了有价值的成果。
We get valuable results about the effect of the stress ratio and residual stress on fatigue crack growth.
19. 疲劳裂纹扩展率表达式是采用疲劳裂纹扩展理论预报疲劳寿命的核心。
The fatigue crack growth rate is the core for predicting fatigue life by use of fatigue crack propagation (FCP) theory.
20. 冷凝器铜管的工作环境使疲劳极限大为降低,加剧了疲劳裂纹的扩展。
The fatigue limit of condenser copper tube was reduced by working condition which aggravated the spread of crack.
21. 由于表面热疲劳裂纹的产生,使得材料强度性能损伤大于断裂韧性损伤。
The strength loss is greaser than the fracture toughness loss, because ofthe surface cracks caused. by thermal fatigue.
22. 讨论了冷轧工作辊接触疲劳裂纹、剥落、夹杂物裂纹和磨损等失效形式。
The failure forms of cold work roll including contact fatigue crack, spalling, inclusion crack and wear are discussed.
23. 本文研究了SCT试样高应变区的疲劳裂纹闭合效应和疲劳裂纹扩展速率。
The fatigue crack closure and fatigue crack growth rate in the high strain region of SCT specimen are studied.
24. 通过分析表明,压应力对裂纹尖端塑性区和疲劳裂纹的扩展有显著的影响。
The analysis shows that the compressive loading has a significant contribution towards the crack tip plasticity and the fatigue crack growth.
25. 疲劳断裂是气门弹簧失效的主要模式,它是疲劳裂纹萌生及其扩展的结果。
The primary failure model is fatigue fracture that is always resulted by the crack initiation and propagation.
26. 本文给出二维疲劳裂纹扩展门槛值分布函数,建立二维应力—门槛值干涉模型。
A distribution function of two dimensional threshold is given for fatigue crack propagation.
27. 结果表明,失效形貌呈典型的接触疲劳特征,两种疲劳裂纹形成模式同时存在。
The results showed that failure morphology was of typical contact fatigue characteristics, and two modes of fatigue crack formation worked.
28. 认为,该曲轴材料的冶金缺陷是导致疲劳裂纹在正常工作应力下过早形成的原因。
The results show that metallurgical defect is the main reason leading to early formation of fatigue crack under normal working stress.
29. 认为,该曲轴材料的冶金缺陷是导致疲劳裂纹在正常工作应力下过早形成的原因。
The results show that metallurgical defect is the main reason leading to early formation of fatigue crack under normal working stress.